Applications: STRUKTOL® V-HRW is a highly compatible, rigid PVC lubricant with both internal and external properties. It is particularly useful in clear PVC articles due to its excellent clarity and low water blush. It can be used in blow molding, injection molding, extrusion and is especially effective in calendaring applications and in products that will be printed, bonded or laminated. Information provided by Struktol Sanctioned for use by the Food and Drug Administration in a number of applications, listed in the following sections of Title 21 of the Code of Federal Regulations:
- 176.170
- 176.210
- 177.1200
- 177.121
- 177.2420
- 178.3280
|