MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol TR 060 Blending Aid, Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: A mixture of light-colored aliphatic resins with a molecular weight below 2,000.

At process temperatures, STRUKTOL® TR 060 melt has a natural tackiness and this "adhesive" nature enables it to act as an effective binder. This is important in polymers where high filler levels require the most uniform blending in order to maintain physical properties. In addition, the low molecular weight of STRUKTOL® TR 060 provides some viscosity reduction during processing which improves flow characteristics.
Many applications require a high level of uniform blending in the initial compounding stage. STRUKTOL® TR 060 has been shown to improve the blending of TPO compounds, flame retardant formulations and filled polymer systems. In many cases, this more homogenous blend results in better physical properties and fewer processing problems. Low level additions of STRUKTOL® TR 060 can be very useful in improving the performance for a range of highly filled compounds. STRUKTOL® TR 060 has good solubility in aliphatic, aromatic and chlorinated hydrocarbons.

FDA Status: 172.280; 172.615; 175.105; 175.125; 175.300; 176.200; 176.210; 177.1200; 177.1210; 177.1350; 177.1390; 177.1520; 177.2600; 178.1005; 178.3750; 178.3850; 178.3930; 179.45

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/cc
Additive Loading 0.50 - 1.0 %0.50 - 1.0 %
Ash 2.0 %2.0 %
 
Thermal PropertiesMetricEnglishComments
Dropping Point 95.0 - 105 °C203 - 221 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 24.0 Month>= 24.0 Month
 
Descriptive Properties
AppearancePale yellow pellets or powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Struktol TR 065 Blending Aid, Processing Additive
Struktol TR 071 Processing Additive
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent
Struktol TPW 604 Processing Additive
Struktol MONTAN WAX E Lubricant, Processing Additive

PSTRUK04 / 69232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.