MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Unsaturated fatty primary amide derived from oleic acid.

One of the major uses of oleamide is as a slip agent in polyethylene films. It functions by migrating to the film surface in a microscopic coating which reduces the coefficient of friction. In general, oleamide migrates more rapidly than erucamide (STRUKTOL® TR 131) but has lesser heat stability. Where this is not a disadvantage, oleamide costs are inherently lower.
This same property of uniform surface bloom permits STRUKTOL® TR 121 to be used in injection molding applications. It functions as both a lubricant and mold release agent. These properties are valuable in processing thermoplastic resins, thermoplastic elastomers (TPEs) and thermoset rubber systems. STRUKTOL® TR 121 may also function as a dispersant in concentrates by providing easier and more uniform letdown of the concentrated material. STRUKTOL® TR 121 is insoluble in water and has limited solubility in alcohols, ketones and aromatic solvents.

FDA Status: 175.105; 175.300; 178.3910; 179.45; 181.28

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Additive Loading 0.050 - 0.50 %0.050 - 0.50 %Applications in the rubber area normally require 1-3 phr loading levels. For plastics, these loading may vary from around 0.05% in films to more than 0.5% in mold release applications
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 3.0<= 3.0
 
Thermal PropertiesMetricEnglishComments
Melting Point 70.0 - 76.0 °C158 - 169 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 4.04.0
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 24.0 Month>= 24.0 Month
 
Descriptive Properties
Amide Content (%)98
AppearanceLight cream colored pellets or beads
Iodine Value (max)90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Struktol TR 065 Blending Aid, Processing Additive
Struktol TR 060 Blending Aid, Processing Additive
Struktol TR 071 Processing Additive
Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent
Struktol CALCIUM STEARATE GR

PSTRUK07 / 69235

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.