MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Unsaturated primary amide derived from erucic acid.

STRUKTOL® TR 131 is mainly used as a slip agent in polyolefin films, reducing the coefficient of friction. It is the agent of choice at higher extrusion temperatures because of its high heat stability and slower rate of migration to the surface compared with oleamides.
The slower rate of migration is also an advantage when films are printed, sealed or laminated shortly after extrusion. Its low odor makes it extremely suitable for food contact applications.
STRUKTOL® TR 131 is also used as a release agent in various polymer systems, and as a dispersant in color concentrates and printing inks. In PVC plastisols for screw closures, it reduces the torque and facilitates release.
STRUKTOL® TR 131 is also used as a process aid or lubricant in thermoplastic elastomers (TPEs), thermoplastic resins and thermoset rubber systems. The properties it imparts to the surface may assist in subsequent operations such as parts assembly.

FDA Status: 175.105; 176.180; 177.1200; 177.1350; 178.3860; 179.45

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/cc
Additive Loading 0.050 - 0.50 %0.050 - 0.50 %For plastics (1-3 phr in elastomers)
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 3.0<= 3.0
 
Thermal PropertiesMetricEnglishComments
Melting Point 79.0 - 85.0 °C174 - 185 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 4.04.0
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 24.0 Month>= 24.0 Month
 
Descriptive Properties
Amide Content (%)99
AppearanceOff-white pellets or beads
Iodine Value (max)78

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Struktol TR 065 Blending Aid, Processing Additive
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent
Struktol TR 060 Blending Aid, Processing Additive
Struktol TR 071 Processing Additive
Struktol CALCIUM STEARATE GR

PSTRUK08 / 69236

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.