MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol TR 065 Blending Aid, Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Blend of medium molecular weight resins designed as a high temperatures process aid and blending agent.

Effective in binding filler materials to the polymer system by virtue of its adhesive nature at process temperatures. The components of STRUKTOL® TR 065 should make it compatible with most polymers, polar or non-polar in nature. It should withstand processing temperatures to 370°C. Those systems, which should benefit from both compounding and processing improvements, include high-filled polyesters, nylon, nitriles, PVC and blends or alloys of dissimilar materials. STRUKTOL® TR 065 is an excellent compatibilizer and has proven useful for processing recycle materials.

FDA Status: 172.280; 172.615; 175.105; 175.125; 175.300; 175.320; 177.2600; 178.3930

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Additive Loading 0.50 - 1.0 %0.50 - 1.0 %
 
Thermal PropertiesMetricEnglishComments
Dropping Point 106 - 116 °C223 - 241 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 24.0 Month>= 24.0 Month
 
Descriptive Properties
AppearanceLight yellow pastilles or powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent
Struktol TR 060 Blending Aid, Processing Additive
Struktol TR 071 Processing Additive
Struktol TR 045 Processing Additive
Struktol TR 044W Processing Additive

PSTRUK05 / 69233

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.