MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colour stability upon weather exposure. This product provides high quality film and good transparency. It is especially designed for high performance extrusion and film processes.

APPLICATIONS: PEARLTHANE® D91F65D is especially recommended for extrusion applications for exterior automotive parts and a variety of high performance technical parts where weather resistance and transparency are required.

Information provided by Merquinsa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65
Tensile Strength, Yield 4351 psiASTM D412
Elongation at Break 372 %ASTM D412
100% Modulus 2.32 ksi
@Strain 100 %
ASTM D412
300% Modulus 3.626 ksi
@Strain 300 %
ASTM D412
Abrasion 40[mm^3]; DIN 53.516
 
Thermal PropertiesOriginal ValueComments
Melting Point 284 - 302 °FMQSA 114
 
Processing PropertiesOriginal ValueComments
Feed Temperature 311 °F
Nozzle Temperature 338 °F
Zone 1 338 - 356 °F
Zone 2 356 - 374 °F
Zone 3 374 - 392 °F
Zone 4 365 - 383 °F
Die Temperature 329 - 347 °F
Mold Temperature 95.0 °F
Moisture Content <= 0.10 %MQSA 44
 
Descriptive Properties
Compression zone320°C
Metering zone320°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer

PMES82a / 109242

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.