MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colour stability upon weather exposure. This product provides high quality film and good transparency. It is especially designed for high performance extrusion and film processes.

APPLICATIONS: PEARLTHANE® D91F65D is especially recommended for extrusion applications for exterior automotive parts and a variety of high performance technical parts where weather resistance and transparency are required.

Information provided by Merquinsa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
10 g/10 min
@Load 47.6 lb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Tensile Strength, Yield 30.00 MPa4351 psiASTM D412
Elongation at Break 372 %372 %ASTM D412
100% Modulus 16.0 MPa
@Strain 100 %
2320 psi
@Strain 100 %
ASTM D412
300% Modulus 25.00 MPa
@Strain 300 %
3626 psi
@Strain 300 %
ASTM D412
Abrasion 4040[mm^3]; DIN 53.516
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 - 150 °C284 - 302 °FMQSA 114
 
Processing PropertiesMetricEnglishComments
Feed Temperature 155 °C311 °F
Nozzle Temperature 170 °C338 °F
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 190 - 200 °C374 - 392 °F
Zone 4 185 - 195 °C365 - 383 °F
Die Temperature 165 - 175 °C329 - 347 °F
Mold Temperature 35.0 °C95.0 °F
Moisture Content <= 0.10 %<= 0.10 %MQSA 44
 
Descriptive Properties
Compression zone320°C
Metering zone320°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer

PMES82a / 109242

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.