MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayfill® EA 2204
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Bayfill EA 2204 is a fully formulated two component system for the production of a friable energy absorbing (EA) foam for interior automotive applications.

Properties / Applications: Bayfill EA 2204 is a fully formulated two component system for the production of a friable energy absorbing (EA) foam for interior automotive applications. The Bayfill EA system is supplied as two components. Component A is a polymeric diphenylmethane diisocyanate (PMDI) and Component B, is a formulated polyether polyol system. As with any product, use of Bayfill EA 2204 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.0450 g/cc0.0450 g/cc
 1.02 g/cc1.02 g/ccPolyol Blend (Component B)
 1.24 g/cc1.24 g/ccIsocyanate (Component A)
Viscosity 200 cP200 cPIsocyanate (Component A)
 2350 cP2350 cPPolyol Blend (Component B)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.164 MPa23.8 psiASTM D3574
Elongation at Break 5.0 %5.0 %ASTM D3574
Compressive Strength 0.198 MPa28.7 psi15% deflection; ASTM D1621
 0.279 MPa40.5 psi20% deflection; ASTM D1621
 
Thermal PropertiesMetricEnglishComments
Flash Point 199 °C390 °FIsocyanate (Component A)
 >= 200 °C>= 392 °FPolyol Blend (Component B)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 57.0 - 63.0 °C135 - 145 °F
Gel Time 0.4167 min0.4167 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baydur® 263 IMR RIM system
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
Covestro SOFTCEL® U-1000 Polyol
Colorite Polymers Vinylbond 6527P-MD Grey 499 Compound

PCOVEST0107 / 201890

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.