MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro SOFTCEL® U-1000 Polyol
Categories: Other Engineering Material

Material Notes: Softcel U-1000 Polyol is a low molecular weight polyol.

Properties / Applications: Softcel U-1000 Polyol is a low molecular weight polyol. It may be used with other slabstock performance polyols from Covestro to produce Softcel V foams, which are characterized by their slow recovery and high damping characteristics. Softcel Polyol U-100 is typically used with Ultracel® 3000 (U-3000) polyol or Arcol® HS-100 polymer polyol to produce Softcel V foams. When properly formulated, these foams exhibit slow yet complete recovery from deformation, low resilience, high vibration damping and body conforming characteristics, which may make them useful in a variety of applications, including mattresses and mattress pads, pillows, furniture, wheelchairs, sports equipment, acoustical panels, gasketing and automotive interiors. As with any product, use of Softcel U-1000 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Bulk Density 1.02 g/cc0.0367 lb/in³
Viscosity  50 cP
@Temperature 60.0 °C
50 cP
@Temperature 140 °F
 200 cP
@Temperature 25.0 °C
200 cP
@Temperature 77.0 °F
 500 cP
@Temperature 15.0 °C
500 cP
@Temperature 59.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 276 °C529 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayfill® EA 2204
Covestro Baydur® 263 IMR RIM system
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
Lendell Manufacturing SRF-1 Foam

PCOVEST0972 / 202755

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.