MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS blends for applications where hard/soft combinations are required. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

Key Features:

  • Designed for excellent adhesion onto ABS, PS, PC, PMMA and ASA (cold insert or 2K [two-shot] molding).
  • Recommended for applications requiring superior part surface appearance.
  • Designed for soft touch applications.
  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Adhesion values can vary according to type of ABS, PS, PC, PMMA, ASA or blends thereof, tool design and processing conditions.
  • EU and China RoHS compliant.
Applications:
  • Automotive – Grips, HVAC Flapper Door Seals, Interior, Electronics, Floor Care, Kitchen Tools, Power Tools, Writing Instruments and Consumer Applications
  • Seals and Gaskets
  • Soft Touch Grips
Uses:
  • Appliance Components
  • Appliances
  • Automotive Applications
  • Automotive Under the Hood
  • Bonding
  • Cell Phones
  • Consumer Applications
  • Eyeglass Frames
  • Flexible Grips
  • Kitchenware
  • Living Hinges
  • Seals
  • Sporting Goods
  • Strain Reliefs
  • Tie-Layer
  • White Goods & Small Appliances
Processing Method: Coextrusion, Injection Molding and Multi Injection Molding

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4949Air at 212°F, 168 hr; ASTM D573
 6161Air at 257°F, 168 hr; ASTM D573
 53
@Thickness 2.00 mm
53
@Thickness 0.0787 in
15 sec; ISO 868
Tensile Strength at Break 1.600 MPa232.1 psiAir at 257°F, 168 hr; ASTM D573
 2.954 MPa428.4 psiAir at 212°F, 168 hr; ASTM D573
 4.10 MPa595 psiAcross Flow; ASTM D412
Tensile Stress at Strain 1.00 MPa
@Strain 100 %
145 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 180 %180 %Air at 257°F, 168 hr; ASTM D573
 516 %516 %Air at 212°F, 168 hr; ASTM D573
 600 %600 %Across Flow; ASTM D412
Compression Set 55 %
@Temperature 125 °C,
Time 252000 sec
55 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -47.0 °C-52.6 °FASTM D746
Flammability, UL94  HB
@Thickness 1.10 mm
HB
@Thickness 0.0433 in
 HB
@Thickness 2.90 mm
HB
@Thickness 0.114 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 98.9 - 110 °C210 - 230 °FFor two-shot injection molding
 110 - 121 °C230 - 250 °FFor insertion injection molding
Mold Temperature 25.0 - 50.0 °C77.0 - 122 °F
 
Descriptive Properties
ColorNatural Color
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
Overview of materials for Polyester Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer

PADVA012 / 22702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.