LR4201R is a natural low-density crosslinkable polyethylene compound. Applications: LR4201R is intended for insulation of XLPE power cables with rated voltages up to 72 kV. Specifications: ISO 1872-PE, KHNX, 23-D022; IEC 60502; IEC 60840; NF C33-223; BS 6622; REA 50-70 (U-1) 87; AEIC CS7; ICEA S-66-524; ICEA S-94-649; ICEA S-93-639; and AEIC CS8-00 (1st edition).Information provided by Borealis AG |