MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis LR4201R Polyethylene Insulation Compound, Crosslinkable  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LR4201R is a natural low-density crosslinkable polyethylene compound. Applications: LR4201R is intended for insulation of XLPE power cables with rated voltages up to 72 kV. Specifications: ISO 1872-PE, KHNX, 23-D022; IEC 60502; IEC 60840; NF C33-223; BS 6622; REA 50-70 (U-1) 87; AEIC CS7; ICEA S-66-524; ICEA S-94-649; ICEA S-93-639; and AEIC CS8-00 (1st edition).

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength at Break >= 13.5 MPaafter aging (168h, 136°C); ASTM D638
 15.0 MPa
Elongation at Break 400 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmDC; ASTM D257
Dielectric Constant 2.3
@Frequency 60000 Hz
ASTM D150
Dielectric Strength >= 22.0 kV/mmASTM D149
Dissipation Factor 0.00050
@Frequency 60000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Hot Set Test, %5150°C, 0.2 MPa;ICEA T-28-562; Permanent Deformation
 75150°C, 0.2 MPa;ICEA T-28-562; Elongation under load

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive
Borealis Casico™ FR4820 Natural Low Smoke Zero Halogen Flame Retardant Insulation Compound for Building Energy Cables
Borealis Borlink™ LS4201S Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LH4201R Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE8280 Polyethylene Insulation Compound, Crosslinkable

PBOREA526 / 108785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.