MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a thin layer extruded on top of the jacket. This compounds permits easy diagnostic testing of the cable to ensure jacket conformity, allowing confirmation of fault-free cable before and after installation. It provides superior environmental stress crack resistance and good electrical conductivity. Due to the semi conductive properties, it will also provide added protection against lightning strikes. Specifications: BS 6622; IEC 60502; and IEC 60840.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.040 %0.040 %Karl Fischer-titration
ESCR 10% Igepal® >= 2.0 hour
@Temperature 50.0 °C
>= 2.0 hour
@Temperature 122 °F
Igepal 10%/Seawater; F0
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45451s; ISO 868
Tensile Strength at Break 3.125 MPa453.2 psiafter aging 240h, 100°C;IEC 60811-1-2
 12.5 MPa1810 psi25mm/min; ISO 527
Elongation at Break 400 %400 %25mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  <= 50 ohm-cm
@Temperature 23.0 °C
<= 50 ohm-cm
@Temperature 73.4 °F
ISO 3915
 <= 1000 ohm-cm
@Temperature 90.0 °C
<= 1000 ohm-cm
@Temperature 194 °F
ISO 3915
 
Processing PropertiesMetricEnglishComments
Zone 1 130 °C266 °F
Zone 2 140 °C284 °F
Zone 3 150 °C302 °F
Zone 4 180 °C356 °F
Die Temperature 180 °C356 °F
Melt Temperature 140 - 180 °C284 - 356 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FL5580 High Density Polyethylene
Borealis Borlink™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis Borlink™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable
Borealis LE6022 Polyethylene Modified Jacketing Compound

PBOREA510 / 108769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.