MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical c-Pentane
Categories: Fluid

Material Notes: Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants or C5 products.

Uses: As a polyurethane foaming agent, it is increasingly used in place of Freon foaming agent.

CAS: 287-92-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.740 - 0.750 g/cc0.740 - 0.750 g/ccASTM D891
Volatiles 100 %
@Temperature 21.0 °C
100 %
@Temperature 69.8 °F
Vapor Pressure 0.424 bar
@Temperature 21.0 °C
318 torr
@Temperature 69.8 °F
Vapor Density=2.42
 
Thermal PropertiesMetricEnglishComments
Melting Point -94.4 °C-138 °F
Boiling Point 49.3 °C
@Pressure 0.101 MPa
121 °F
@Pressure 14.7 psi
Flash Point >= -7.00 °C>= 19.4 °F
Ignition Temperature 361 °C682 °FAutoignition
 
Descriptive Properties
ComponentsBENZENE<5 ppm
 BUTANE0.05%
 Cyclopentane>95%
 CYCLO-PENTANE>95%
 I-HEXANE<3 ppm
 Iso/n-pentane<3%
 Iso-hexane<3%
 ISO-PENTANE<3%
 N-HEXANE<20 ppm
 N-PENTANE<3%
 WATER<50 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 612 Magnesium Protection Fluid
3M Fluorinert™ FC-72 Electronic Liquid
Wacker Wacker® Methyl acetate 97%
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (31 wt% - 36 wt% Concentration)
Solvay Chemicals 38% Technical Grade Hydrochloric acid

PLAY781 / 148791

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.