MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Chemicals 38% Technical Grade Hydrochloric acid
Categories: Fluid

Material Notes: Property data for 38 wt% aqueous solution of HCl. Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regenerating, pickling or cleaning agent.

EINECS: 231-595-7/CAS: 7647-01-0/UN: 1789

Information provided by Solvay

Key Words: Muriatic Acid
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.1393 g/cc
@Temperature 100 °C
0.041160 lb/in³
@Temperature 212 °F
 1.1754 g/cc
@Temperature 40.0 °C
0.042464 lb/in³
@Temperature 104 °F
 1.2156 g/cc
@Temperature -5.00 °C
0.043916 lb/in³
@Temperature 23.0 °F
Molecular Weight 36.47 g/mol36.47 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point -28.0 °C-18.4 °F
Boiling Point 45.0 °C
@Pressure 0.101 MPa
113 °F
@Pressure 14.6 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 612 Magnesium Protection Fluid
3M Fluorinert™ FC-72 Electronic Liquid
3M Novec™ 1230 Fire Protection Fluid
Wacker Wacker® Methyl acetate 97%
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (31 wt% - 36 wt% Concentration)

WSOLV138 / 147787

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.