MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Wacker® Methyl acetate 97%
Categories: Fluid

Material Notes: Empirical formula: C3H6O2

CAS No.: 79-20-9

Product description: WACKER® Methyl acetate 97% is a clear, colorless, neutral liquid with a mild, ester-like odor. Methyl acetate is one of the best solvents available. It is used predominantly for dyes and in the coatings, adhesives, cosmetics, plant-protection and pharmaceutical industries.

Application:

  • parquet Adhesives
  • all Purpose Adhesives
  • interior Paints
  • solvent for chemical Industries

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³
Vapor Pressure  0.200 bar
@Temperature 20.0 °C
150 torr
@Temperature 68.0 °F
 0.900 bar
@Temperature 50.0 °C
675 torr
@Temperature 122 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point -100 °C-148 °F
Boiling Point 54.0 - 57.0 °C
@Pressure 0.1013 MPa
129 - 135 °F
@Pressure 14.69 psi
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Content<0.9%Acetaldehyde
 <2.9%Methanol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Fluorinert™ FC-72 Electronic Liquid
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (31 wt% - 36 wt% Concentration)
Solvay Chemicals 38% Technical Grade Hydrochloric acid
LG Chemical c-Pentane
Evonik DRIVERON® MTBE Liquid

PWACK9791 / 205320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.