MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milAdhesive
 3.20 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 3.4375 pliLDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
 3.75 pliLDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
 4.0625 pliHDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
 4.375 pliHDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
 6.25 pliPolypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
 6.25 pliPolypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
 6.25 pliPolypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
 6.25 pliPolypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
 7.50 pliPolypropylene, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
 8.125 pliPolypropylene, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
 8.125 pliABS, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
 8.75 pliStainless Steel, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
 8.75 pliPolycarbonate, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
 8.75 pliPolycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
 8.75 pliABS, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
 8.75 pliStainless Steel, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
LinerNatural, 60#

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade
Eastman 1840A Polyethylene
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
Bamberger Polymers Bapolene® 1030 Low Density Polyethylene Extrusion/Injection Resin
Armacell OleTex® BKJN 200 LDPE Foam

PMM33243 / 167990

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.