MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Applications
The PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized products offer excellent additive homogeneity, require no transfer equipment modifications and facilitate clean and safe storage and handling. They can be used in either blown or cast film extrusion. GA 502-024 is specifically formulated with extra antioxidant for use in cast film. It contains no other additives.

Processing Techniques
GA 502 series resins exhibit excellent drawdown characteristics. Recommended conditions are 375-425°F melt temperature and a 1.5-3.0:1 blow-up ratio. Using proper techniques, these products can readily be drawn below .5 mil at optimum production rates. Specific recommendations for type of resin and extrusion conditions can be made only when the end use, required properties and processing equipment are known.

Regulatory Status
GA 502 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520, Subpart C, Item 3.1. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

Other Information
Blow-Up ratio 2.1:1, Anti-Block level, ppm, High.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Thickness 38.1 microns1.50 mil2:1 BUR
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 750 %750 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Coefficient of Friction <= 0.20<= 0.20ASTM D1894
Elmendorf Tear Strength MD 170 g170 gASTM D1922
Elmendorf Tear Strength TD 400 g400 gASTM D1922
Dart Drop Test 120 g0.265 lbF50; ASTM D1709A
Film Tensile Strength at Break, MD 33.8 MPa4900 psiASTM D882
Film Tensile Strength at Break, TD 24.8 MPa3600 psiASTM D882
1% Secant Modulus, MD 221 MPa32000 psiASTM D638
1% Secant Modulus, TD 248 MPa36000 psiASTM D638
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 60 %60 %ASTM D523
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AntiblockHigh
Slip LevelHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene
LyondellBasell Petrothene® GA501022 Linear Low Density Polyethylene
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene

PEQU0338 / 36776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.