System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360
Categories:
Polymer
;
Adhesive
Material Notes:
3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Thickness
50.8
microns
2.00
mil
Adhesive
81.3
microns
3.20
mil
Liner
Mechanical Properties
Metric
English
Comments
Peel Strength
0.60259
kN/m
3.4375
pli
LDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
0.657
kN/m
3.75
pli
LDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
0.71216
kN/m
4.0625
pli
HDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
0.7669
kN/m
4.375
pli
HDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.10
kN/m
6.25
pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
1.10
kN/m
6.25
pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
1.10
kN/m
6.25
pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
1.10
kN/m
6.25
pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
1.31
kN/m
7.50
pli
Polypropylene, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.424
kN/m
8.125
pli
Polypropylene, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.424
kN/m
8.125
pli
ABS, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.53
kN/m
8.75
pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.53
kN/m
8.75
pli
Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.53
kN/m
8.75
pli
Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.53
kN/m
8.75
pli
ABS, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.53
kN/m
8.75
pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
Processing Properties
Metric
English
Comments
Shelf Life
24.0
Month
24.0
Month
Descriptive Properties
Liner
Natural, 60#
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade
Eastman 1840A Polyethylene
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
Bamberger Polymers Bapolene® 1030 Low Density Polyethylene Extrusion/Injection Resin
Armacell OleTex® BKJN 200 LDPE Foam
PMM33243 / 167990
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.