Supercure™ LE8201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Supercure™ LE8201R is recommended for use with Supercure™ LE8280 as shielding compound. Applications: Supercure LE8201R is intended for insulation of XLPE power cables with rated voltages up to 72 kV. Specifications: Supercure™ LE8201R meets these applicable requirements when processed using sound extrusion practice and testing procedure: AEIC CS8; HD 620 S1, Part 1, table 2A, DIX 3 to 14; and IEC 60502.Information provided by Borealis AG |