MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Syncure™ systems are two part moisture crosslinkable compounds. S112NA is a CSA listed, high strength, colorable power cable insulation compound and RoHS compliant.

NOTE: Typical Properties measured on 14 AWG with 30 mil wall. STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
Deformation 10 %
@Temperature 131 °C,
Time 3600 sec
10 %
@Temperature 268 °F,
Time 1.00 hour
500 g; UL 1581
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 474710 sec; ASTM D2240
 5353ASTM D2240
Tensile Strength, Yield 19.3 MPa2800 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 400 %400 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.24
@Frequency 1e+6 Hz
2.24
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 39.0 kV/mm991 kV/inASTM D149
Dissipation Factor 0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
ASTM D150
 
Descriptive Properties
Agency RatingsCSA C-22.2 0.3
 IEC 60502
AppearanceNatural Color
Catalyst Masterbatch5%S-1000B
FeaturesIndustrial Resin
FormsPellets
Gel Content72%ASTM D2765; Crosslinked PE, Method B (NonReferee Test)
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Grafted Base Resin95%S-1054A
Processing MethodExtrusion Coating
Regional AvailabilityNorth America
Retention of Tensile Elongation90%121°C, 1.91 mm; 336 hr, UL Standard
Retention of Tensile Strength95%121°C, 1.91 mm; 336 hr, UL Standard
UsesWire & Cable Applications
Wire TypesNMD90
 RW-90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis LE4212L Polyethylene Insulation Compound, Crosslinkable
Syensqo (Solvay Specialty Polymers) Polidan® T/A Polyethylene, Crosslinked (XLPE)
Avient Syncure™ V0045G RoHS Polyethylene, Crosslinked (XLPE)
Borealis Borlink™ LH4201R Polyethylene Insulation Compound, Crosslinkable
Avient FireCon™ CPE 37-11 RoHS BLACK Polyethylene, Chlorinated (CPE)

PH0POL0293 / 144862

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.