MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Syncure™ V0045G RoHS Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.

Gel, Torque, Dispersion, and Oven Aging were measured on a 100 phr S1025A / 50 phr V0045G Syncure System. Cured for 6 hours in water at 90°C for Gel test and Oven Aging. Torque is > 1400. Dispersion is Visual. Pellet appearance is 1/8 round.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/ccASTM D792
Density 1.00 g/cc0.0361 lb/in³Geon® 1169; Internal Method
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Gel Content60%ASTM D2765; Crosslinked PE, Method A (Referee Test)
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Regional AvailabilityNorth America
Retention of Tensile Elongation80%158°C, 1.91 mm; 672 hr, UL Standard
Retention of Tensile Strength85%158°C, 1.91 mm; 672 hr, UL Standard
RoHS ComplianceRoHS Compliant
UsesWire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Syncure™ V0022G Crosslinked Polyethylene (XLPE)
Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Avient FireCon™ CPE 1240 UV RoHS NATURAL Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE 37-11 RoHS BLACK Polyethylene, Chlorinated (CPE)
Borealis Borlink™ LH4201R Polyethylene Insulation Compound, Crosslinkable

PH0POL0337 / 144906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.