MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3WG3 BK 00564 15% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be given to the grades A3Eg3 and A3hg3

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.23 g/ccISO 1183
Moisture Absorption at Equilibrium 1.9 - 2.5 %23°C; 50% RH; ISO 62
 2.2 %50% RH; ISO 62
 7.0 %Saturation; ISO 62
Water Absorption at Saturation 6.7 - 7.3 %ISO 62
Viscosity Measurement 145ISO 307
Linear Mold Shrinkage 0.0075 cm/cmrestricted
Melt Flow 73.8 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaISO 527
Tensile Strength, Yield 130 MPa50 mm/min; ISO 527-1/-2
Elongation at Break 2.5 %ISO 527
Elongation at Yield 3.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 6.00 GPaISO 527-1/-2
Flexural Strength 200 MPaat max force; ISO 178
Flexural Modulus 5500 MPaISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 43.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 450 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 - 35.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
CTE, linear, Transverse to Flow 70.0 - 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
Thermal Conductivity 0.330 W/m-KDIN 52612
Melting Point 260 °CDIN 53765
Maximum Service Temperature, Air 145 °Cfor 50% loss of tensile strength after 20000hr
 175 °Cfor 50% loss of tensile strength after 5000hr
 240 °C
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75-1/-2
Decomposition Temperature >= 310 °C
 >= 310 °C
Flammability, UL94 HB
@Thickness 1.60 mm
Ignition Temperature >= 400 °CASTM D1929
 >= 400 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 290 °CFeed zone
Zone 2 290 °CCompression
Zone 3 290 °CMetering-zone
Zone 4 290 °CNozzle
Melt Temperature 280 - 300 °CInjection-molding/Extrusion
 290 °COptimal
Mold Temperature 80.0 °COptimal
 80.0 - 90.0 °CInjection-molding
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
ColorBK 00564
Commercial StatusEurope and North America
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SSAB Tunnplat Docol® 1000 DP High-strength Steel
BASF Ultramid® A3WG3 BK 00564 15% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned)

PBASG0232 / 131865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.