MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3WG3 BK 00564 15% Glass Filled PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be given to the grades A3Eg3 and A3hg3

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.9 - 2.5 %1.9 - 2.5 %23°C; 50% RH; ISO 62
 2.2 %2.2 %50% RH; ISO 62
 7.0 %7.0 %Saturation; ISO 62
Water Absorption at Saturation 6.7 - 7.3 %6.7 - 7.3 %ISO 62
Viscosity Measurement 145145ISO 307
Linear Mold Shrinkage 0.0075 cm/cm0.0075 in/inrestricted
Melt Flow 73.8 g/10 min
@Load 5.00 kg,
Temperature 275 °C
73.8 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.0 MPa12300 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 10 %10 %50mm/min; ISO 527-1/-2
Modulus of Elasticity 4.50 GPa653 ksiISO 527-1/-2
Flexural Strength 125 MPa18100 psiat max force; ISO 178
Flexural Modulus 4.00 GPa580 ksiISO 178
Izod Impact, Notched (ISO) 5.60 kJ/m²
@Temperature 23.0 °C
2.66 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 2600 MPa
@Strain <=0.5 %
377000 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.5
@Frequency 1e+6 Hz
5.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.30
@Frequency 1e+6 Hz
0.30
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 450 V450 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.330 W/m-K2.29 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 145 °C293 °Ffor 50% loss of tensile strength after 20000hr
 175 °C347 °Ffor 50% loss of tensile strength after 5000hr
 240 °C464 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 290 °C554 °FFeed zone
Zone 2 290 °C554 °FCompression
Zone 3 290 °C554 °FMetering-zone
Zone 4 290 °C554 °FNozzle
Melt Temperature 280 - 300 °C536 - 572 °FInjection-molding/Extrusion
 290 °C554 °FOptimal
Mold Temperature 80.0 °C176 °FOptimal
 80.0 - 90.0 °C176 - 194 °FInjection-molding
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
ColorBK 00564
Commercial StatusEurope and North America
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3WG3 BK 00564 15% Glass Filled PA66 (Dry)
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)

PBASG0233 / 131866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.