MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SSAB Tunnplat Docol® 1000 DP High-strength Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: High-strength Steel

Characteristics: The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel is heated to 200-400°C and then acquires its final structure to which the steel owes it toughness and good formability. This unique annealing procedure produces a tempered martensitic structure that accounts for the high strength of the steel. Both annealing and tempering are carried out in an inert atmosphere to prevent the steel from oxidizing, and the steel strip runs through a pickling bath between quenching and tempering, in order to remove the thin oxide film formed in the quenching process.

Comments: Docol - Cold Rolled Steel - Ultra high-strength steel (UHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm.

Applications: Tubes, Transport cages, Child seats for cars, Truck load stays, Venetian blinds, Washers, Hose clips, Clutch plates, Hedge cutters, Springs, Spades, Safes, Knives, Train seats, Ladders, Circlips, Saw blades, Chains, Bumpers, Bicycles, Containers, Clips

Data provided by SSAB Tunnplat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1000 - 1200 MPa145000 - 174000 psi
Tensile Strength, Yield >= 850 MPa>= 123000 psiAfter bake hardening
 700 - 950 MPa
@Strain 0.2 %
102000 - 138000 psi
@Strain 0.2 %
Elongation at Break >= 5.0 %>= 5.0 %A80
Bend Radius, Minimum >= 3.0 t>= 3.0 t90° bend
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.040 %0.040 %
Carbon, C 0.15 %0.15 %
Iron, Fe 98 %98 %As remainder
Manganese, Mn 1.5 %1.5 %
Niobium, Nb (Columbium, Cb) 0.015 %0.015 %
Phosphorus, P 0.015 %0.015 %
Silicon, Si 0.50 %0.50 %
Sulfur, S 0.0020 %0.0020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SSAB Tunnplat Docol® 1000 DL High-strength Steel
BASF Ultramid® A3WG3 BK 00564 15% Glass Filled PA66 (Dry)
AISI 5135 Steel
AISI 1034 Steel
SSAB Tunnplat Docol® 1200 DP High-strength Steel

NTUNN49 / 19541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.