MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Struktol TR 141 Slip Agent, Lubricant, Mold Release Agent
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: A saturated primary amide with no double bond.

STRUKTOL® TR 141 stearamide is a saturated primary amide with no double bond. It blooms in an invisible monolayer for surface appearance and mold release. It can also be used for viscosity reduction.
STRUKTOL® TR 141 is relatively insoluble in water and has limited solubility in alcohol, ketones and aromatic solvents. STRUKTOL® TR 141 will not interfere with peroxide cure systems in cross-linked polymer systems.

FDA Status: 175.105; 177.1210; 178.3910; 179.45; 181.28

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/cc
Additive Loading 0.50 - 1.0 %For plastics (1-3 phr in elastomers)
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 9.0
 
Thermal PropertiesOriginal ValueComments
Melting Point 98.0 - 104 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 5.0
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 24.0 Month
 
Descriptive Properties
AppearanceCream colored beads or pellets.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent
BYK ADD-VANCE® SA 155 Slip Masterbatch, PP homopolymer base
Struktol TR 255 Processing Additive, Dispersant
Struktol TR 251 Processing Additive, Dispersant

PSTRUK09 / 69237

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.