MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel
Categories: Metal; Electronic/Magnetic Alloy

Material Notes: Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard grades from M-15 to M-47 are available with the advantages of special DI-MAX® processing that enhance the magnetic properties.

DI-MAX grades have superior permeability at high inductions, low average core loss and good gauge uniformity. In addition, cold finishing plus strip annealing produce a smooth surface and reduce buckles and waves, resulting in excellent flatness and a high stacking factor.

AK Steel Nonoriented Electrical Steels are available both Fully Processed and Semi-Processed, depending on grade. Properties of Fully Processed material are developed completely by AK Steel. These materials are ready for use without any additional processing required. However, a low-temperature heat treatment may be employed by the user to eliminate stresses introduced by fabrication of the material into cores. AK Steel Fully Processed Nonoriented Electrical Steels meet all the requirements of ASTM Specification A 677.

Semi-Processed steels are finished to final thickness and physical form by AK Steel, but are not fully annealed to develop final magnetic quality. With these materials, achievement of magnetic properties becomes the responsibility of the user. AK Steel Semi-Processed Nonoriented Electrical Steels meet all requirements of ASTM A 683.

DI-MAX M-15 is Fully Processed.

Applications for M-15: Large Motors and Generators (>100 HP)

Information provided by AK Steel

Key Words: ASTM A677
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 72
Tensile Strength, Ultimate 71000 psi
Tensile Strength, Yield 52000 psi
Elongation at Break 23 %in 2"
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000500 ohm-cm
 
Magnetic PropertiesOriginal ValueComments
Core Loss 1.45 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
0.014"; ASTM A677
 1.60 W/lb
@Magnetic Field 1.50 T,
Frequency 60 Hz
0.0185"; ASTM A677
 
Descriptive Properties
Coercive Force (Oe)0.41Bmax =10kG
Hysteresis loss (J/lb/cycle)0.0068Bmax =10kG
Maximum Permeability8000
Saturation Induction Kilogausses20.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel DI-MAX® M-19 Nonoriented Electrical Steel
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)
AK Steel DI-MAX® M-22 Nonoriented Electrical Steel
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel (Extended Electrical/Magnetic Data)
AK Steel DI-MAX® M-27 Nonoriented Electrical Steel

NAKS154 / 139293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.