Physical Properties | Original Value | Comments |
---|
Density | 1.00 - 4.00 g/cc |
| 0.880 - 0.970 g/cc @Temperature 220 - 325 °C |
Filler Content | 15.0 - 60.0 % |
Water Absorption | 0.0600 - 9.50 % |
Moisture Absorption at Equilibrium | 0.170 - 8.00 % |
| 2.00 - 2.60 % @Temperature 70.0 - 70.0 °C |
Water Absorption at Saturation | 4.90 - 10.0 % |
Viscosity | 440000 - 440000 cP @Temperature 280 - 280 °C |
| 440000 - 440000 cP @Shear Rate 1000 - 1000 1/s |
Viscosity Test | 125 - 150 cm³/g |
Maximum Moisture Content | 0.0200 - 0.200 |
| 0.200 - 0.200 @Temperature 120 - 120 °C |
| 0.200 - 0.200 @Time 299 - 299 sec |
Linear Mold Shrinkage | 0.000100 - 0.0350 cm/cm |
| 0.0120 - 0.0130 cm/cm @Temperature 80.0 - 80.0 °C |
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0253 cm/cm |
| 0.0130 - 0.0150 cm/cm @Temperature 80.0 - 80.0 °C |
Melt Flow | 3.00 - 121 g/10 min |
Spiral Flow | 60.0 - 85.0 cm |
|
Mechanical Properties | Original Value | Comments |
---|
Hardness, Rockwell M | 60.0 - 85.0 |
Hardness, Rockwell R | 40.0 - 125 |
| 114 - 114 @Temperature 80.0 - 80.0 °C |
Hardness, Shore D | 47.0 - 82.0 |
Ball Indentation Hardness | 30.0 - 220 MPa |
Tensile Strength, Ultimate | 12.0 - 470 MPa |
| 68.0 - 100 MPa @Temperature -40.0 - -40.0 °C |
Tensile Strength, Yield | 25.0 - 207 MPa |
| 12.0 - 117 MPa @Temperature -40.0 - 120 °C |
Elongation at Break | 1.50 - 500 % |
| 5.50 - 21.5 % @Temperature -40.0 - 150 °C |
Elongation at Yield | 2.10 - 350 % |
| 4.00 - 37.0 % @Temperature -40.0 - 120 °C |
Modulus of Elasticity | 0.150 - 1090 GPa |
| 0.145 - 3.30 GPa @Temperature -40.0 - 150 °C |
Flexural Yield Strength | 9.65 - 310 MPa |
| 8.00 - 148 MPa @Temperature -40.0 - 120 °C |
Flexural Modulus | 0.0689 - 14.0 GPa |
| 0.145 - 2.60 GPa @Temperature -40.0 - 120 °C |
Flexural Strain at Break | 3.70 - 9.00 % |
Compressive Yield Strength | 24.0 - 125 MPa |
Poissons Ratio | 0.350 - 0.470 |
Izod Impact, Notched | 0.0850 J/cm - NB |
| 0.350 - 7.30 J/cm @Temperature -40.0 - -20.0 °C |
| 0.588399 - 5338.47 J/cm @Temperature -40.0 - -20.0 °C |
| 0.588399 - 5338.47 J/cm @Thickness 3.17 - 6.40 mm |
Izod Impact, Unnotched | 13.9 J/cm - NB |
Izod Impact, Notched (ISO) | 4.00 kJ/m² - NB |
| 5.00 - 85.0 kJ/m² @Temperature -40.0 - -30.0 °C |
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² - NB |
| 40.0 kJ/m² - NB @Temperature -30.0 - -30.0 °C |
Charpy Impact Unnotched | 0.450 J/cm² - NB |
| 4.00 J/cm² - NB @Temperature -70.0 - -20.0 °C |
Charpy Impact, Notched | 0.400 J/cm² - NB |
| 0.300 - 2099.79 J/cm² @Temperature -40.0 - -20.0 °C |
Gardner Impact | 36.2 J |
Dart Drop, Total Energy | 45.0 - 45.0 J @Temperature -20.0 - -20.0 °C |
Puncture Energy | 16.0 - 64.0 J |
| 25.0 - 64.0 J @Temperature -30.0 - -30.0 °C |
| 64.0 - 64.0 J @Temperature -30.0 - -30.0 °C |
| 64.0 - 64.0 J @Load <=5810 kg |
Taber Abrasion, mg/1000 Cycles | 6.00 - 19.0 |
|
Electrical Properties | Original Value | Comments |
---|
Electrical Resistivity | 100 - 1.00e+16 ohm-cm |
Surface Resistance | 100 - 1.00e+15 ohm |
Dielectric Constant | 2.70 - 15.4 |
Dielectric Strength | 11.8 - 100 kV/mm |
Dissipation Factor | 0.00300 - 0.400 |
Dielectric Loss Index | 0.0190 - 0.300 |
Arc Resistance | 113 - 195 sec |
Comparative Tracking Index | 400 - 600 V |
|
Thermal Properties | Original Value | Comments |
---|
CTE, linear | 7.00 - 200 µm/m-°C |
| 91.0 - 91.0 µm/m-°C @Temperature 55.0 - 160 °C |
CTE, linear, Transverse to Flow | 50.0 - 190 µm/m-°C |
| 86.0 - 86.0 µm/m-°C @Temperature 55.0 - 160 °C |
Specific Heat Capacity | 1.50 - 3.89 J/g-°C |
| 2.22 - 2.60 J/g-°C @Temperature 270 - 325 °C |
Thermal Conductivity | 0.168 - 0.320 W/m-K |
| 0.150 - 0.180 W/m-K @Temperature 270 - 325 °C |
Melting Point | 205 - 300 °C |
Maximum Service Temperature, Air | 55.0 - 200 °C |
Hot Ball Pressure Test | 125 - 165 °C |
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 - 221 °C |
Deflection Temperature at 1.8 MPa (264 psi) | 35.0 - 213 °C |
Deflection Temperature at 8.0 MPa | 40.0 - 125 °C |
Vicat Softening Point | 95.0 - 225 °C |
Minimum Service Temperature, Air | -100 - -40.0 °C |
Glass Transition Temp, Tg | 0.000 - 60.0 °C |
UL RTI, Electrical | 60.0 - 65.0 °C |
UL RTI, Mechanical with Impact | 60.0 - 65.0 °C |
UL RTI, Mechanical without Impact | 60.0 - 65.0 °C |
Flammability, UL94 | HB - V-0 |
Flame Spread | 10.0 - 100 mm/min |
Oxygen Index | 21.0 - 23.0 % |
Glow Wire Test | 650 - 850 °C |
|
Processing Properties | Original Value | Comments |
---|
Processing Temperature | 221 - 300 °C |
Nozzle Temperature | 230 - 299 °C |
Melt Temperature | 210 - 330 °C |
Mold Temperature | 21.1 - 120 °C |
Drying Temperature | 60.0 - 120 °C |
Moisture Content | 0.000 - 0.200 % |
Dew Point | -40.0 - -17.8 °C |
Injection Pressure | 4.14 - 150 MPa |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.