MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tritan™ FX100 Copolyester
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed without pre-drying and with a wide processing window that allows for product designs that reflect intricate detail.

Application/Uses

  • Consumer and durable goods
  • Graphic arts
  • Leisure and safety
  • Specialty films

Key Attributes

  • Does not contain Bisphenol-A (BPA)
  • Does not contain plasticizers
  • Excellent clarity
  • Good heat resistance
  • No pre-drying of film prior to thermoforming
  • Outstanding chemical resistance
  • Good toughness
  • Wide thermoforming window

Information was provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D1505
Water Absorption 0.50 %
@Time 86400 sec
ASTM D570
Water Vapor Transmission 4.00 g/m²/day
@Temperature 23.0 °C
ASTM F1249
 11.0 g/m²/day
@Temperature 38.0 °C
ASTM F1249
Oxygen Transmission 32.0 cc-mm/m²-24hr-atmASTM D3985
Carbon Dioxide Transmission 149 cc-mm/m²-24hr-atmASTM D1434
Thickness 254 micronsThickness of film tested; ASTM D374
Surface Tension 8.0 dynes/cmPolar; ASTM D5946
 39 dynes/cmDispersive; ASTM D5946
 46 dynes/cmTotal; ASTM D5946
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 41.0 MPaASTM D882
Film Tensile Strength at Yield, TD 40.0 MPaASTM D882
Film Elongation at Break, MD 179 %ASTM D882
Film Elongation at Break, TD 203 %ASTM D882
Film Elongation at Yield, MD 7.0 %ASTM D882
Film Elongation at Yield, TD 7.0 %ASTM D882
Secant Modulus, MD 1.50 GPaTangent; ASTM D882
Secant Modulus, TD 1.40 GPaTangent; ASTM D882
Puncture Energy 4.60 JDynatup; ASTM D3763
Tear Strength 11.0 kN/mMD; Trouser @200/mm/min; ISO 6383-1
 11.0 kN/mTD; Trouser @200/mm/min; ISO 6383-1
 12.0 kN/mSplit tear method, TD; ASTM D1938
 13.0 kN/mSplit tear method, MD; ASTM D1938
Elmendorf Tear Strength MD 520 gASTM D1922
Elmendorf Tear Strength TD 571 gASTM D1922
Elmendorf Tear Strength, MD 2.00 g/micronASTM D1922
Elmendorf Tear Strength, TD 2.20 g/micronASTM D1922
Dart Drop 3.50 g/micron
@Temperature 23.0 °C
ASTM 1709A
 3.60 g/micron
@Temperature -30.0 °C
ASTM 1709A
Dart Drop Test 882 g
@Temperature 23.0 °C
ASTM 1709A
 913 g
@Temperature -30.0 °C
ASTM 1709A
Film Tensile Strength at Break, MD 59.0 MPaASTM D882
Film Tensile Strength at Break, TD 52.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM D696
Specific Heat Capacity 0.410 BTU/lb-°F
@Temperature 60.0 °C
DSC
 0.450 BTU/lb-°F
@Temperature 100 °C
DSC
 0.540 BTU/lb-°F
@Temperature 150 °C
DSC
 0.580 BTU/lb-°F
@Temperature 200 °C
DSC
 0.620 BTU/lb-°F
@Temperature 250 °C
DSC
Glass Transition Temp, Tg 110 °CDSC
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.55ASTM D542
Haze 0.70 %ASTM D1003
Gloss 161 %@ 60°; ASTM D2457
Yellow Index 0.50 %ASTM D1925
Transmission, Visible 92 %ASTM D1003
UV Transmittance 89 %
@Thickness 0.380 mm
UV/Vis Spectro
 
Compliance PropertiesOriginal ValueComments
FDA YesRepeated use food contact articles
NSF YesFood equipment materials; NSF/ANSI Standard 51
 
Descriptive Properties
PPT Tear Resistance, M.D.42 NASTM D2582
PPT Tear Resistance, T.D.56 NASTM D2582
Taber Abrasion23% hazeASTM 1044, Average at 25 cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tritan™ MP100 Copolyester
Eastman Tritan™ EX401 Copolyester
Eastman Tritan™ GX100 Copolyester
Eastman Tritan™ TX1000 Copolyester
Eastman Tritan™ FX200 Copolyester

PE8908 / 109250

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.