MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Tritan™ FX200 Copolyester
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed without pre-drying and with a wide processing window that allows for product designs that reflect intricate detail.

Application/Uses

  • Consumer and durable goods
  • Graphic arts
  • Leisure and safety
  • Specialty films

Key Attributes

  • Does not contain Bisphenol-A (BPA)
  • Does not contain plasticizers
  • Excellent clarity
  • Very good heat resistance
  • No pre-drying of film prior to thermoforming
  • Good chemical resistance
  • Good toughness
  • Wide thermoforming window

Information was provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D1505
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
ASTM D570
Water Vapor Transmission  4.00 g/m²/day
@Temperature 23.0 °C
0.258 g/100 in²/day
@Temperature 73.4 °F
ASTM F1249
 10.0 g/m²/day
@Temperature 38.0 °C
0.644 g/100 in²/day
@Temperature 100 °F
ASTM F1249
Oxygen Transmission 44.0 cc-mm/m²-24hr-atm112 cc-mil/100 in²-24hr-atmASTM D3985
Carbon Dioxide Transmission 211 cc-mm/m²-24hr-atm536 cc-mil/100 in²-24hr-atmASTM D1434
Thickness 254 microns10.0 milThickness of film tested; ASTM D374
Surface Tension 8.0 dynes/cm8.0 dynes/cmPolar; ASTM D5946
 39 dynes/cm39 dynes/cmDispersive; ASTM D5946
 47 dynes/cm47 dynes/cmTotal; ASTM D5946
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 43.0 MPa6240 psiASTM D882
Film Tensile Strength at Yield, TD 41.0 MPa5950 psiASTM D882
Film Elongation at Break, MD 114 %114 %ASTM D882
Film Elongation at Break, TD 115 %115 %ASTM D882
Film Elongation at Yield, MD 8.0 %8.0 %ASTM D882
Film Elongation at Yield, TD 8.0 %8.0 %ASTM D882
Secant Modulus, MD 1.50 GPa218 ksiTangent; ASTM D882
Secant Modulus, TD 1.40 GPa203 ksiTangent; ASTM D882
Puncture Energy 4.50 J3.32 ft-lbDynatup; ASTM D3763
Tear Strength 9.00 kN/m51.4 pliTD; Trouser @200/mm/min; ISO 6383-1
 9.00 kN/m51.4 pliSplit tear method, TD; ASTM D1938
 10.0 kN/m57.1 pliMD; Trouser @200/mm/min; ISO 6383-1
 10.0 kN/m57.1 pliSplit tear method, MD; ASTM D1938
Elmendorf Tear Strength MD 377 g377 gASTM D1922
Elmendorf Tear Strength TD 428 g428 gASTM D1922
Elmendorf Tear Strength, MD 1.50 g/micron38.1 g/milASTM D1922
Elmendorf Tear Strength, TD 1.70 g/micron43.2 g/milASTM D1922
Dart Drop  3.20 g/micron
@Temperature 23.0 °C
81.3 g/mil
@Temperature 73.4 °F
ASTM 1709A
 3.20 g/micron
@Temperature -18.0 °C
81.3 g/mil
@Temperature -0.400 °F
ASTM 1709A
 3.20 g/micron
@Temperature -30.0 °C
81.3 g/mil
@Temperature -22.0 °F
ASTM 1709A
Dart Drop Test  825 g
@Temperature 23.0 °C
1.82 lb
@Temperature 73.4 °F
ASTM 1709A
 825 g
@Temperature -18.0 °C
1.82 lb
@Temperature -0.400 °F
ASTM 1709A
 852 g
@Temperature -30.0 °C
1.88 lb
@Temperature -22.0 °F
ASTM 1709A
Film Tensile Strength at Break, MD 57.0 MPa8270 psiASTM D882
Film Tensile Strength at Break, TD 42.0 MPa6090 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696
Specific Heat Capacity  1.76 J/g-°C
@Temperature 60.0 °C
0.420 BTU/lb-°F
@Temperature 140 °F
DSC
 1.92 J/g-°C
@Temperature 100 °C
0.460 BTU/lb-°F
@Temperature 212 °F
DSC
 2.26 J/g-°C
@Temperature 150 °C
0.540 BTU/lb-°F
@Temperature 302 °F
DSC
 2.43 J/g-°C
@Temperature 200 °C
0.580 BTU/lb-°F
@Temperature 392 °F
DSC
 2.59 J/g-°C
@Temperature 250 °C
0.620 BTU/lb-°F
@Temperature 482 °F
DSC
Glass Transition Temp, Tg 119 °C246 °FDSC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54ASTM D542
Haze 0.80 %0.80 %ASTM D1003
Gloss 158 %158 %@ 60°; ASTM D2457
Yellow Index 0.50 %0.50 %ASTM D1925
Transmission, Visible 93 %93 %ASTM D1003
UV Transmittance 89 %
@Thickness 0.380 mm
89 %
@Thickness 0.0150 in
UV/Vis Spectro
 
Compliance PropertiesMetricEnglishComments
FDA YesYesRepeated use food contact articles
NSF YesYesFood equipment materials; NSF/ANSI Standard 51
 
Descriptive Properties
PPT Tear Resistance, M.D.40 NASTM D2582
PPT Tear Resistance, T.D.40 NASTM D2582
Taber Abrasion20% hazeASTM 1044, Average at 25 cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ MP100 Copolyester
Eastman Tritan™ FX100 Copolyester
Eastman Tritan™ TX2000 Copolyester
Eastman Tritan™ GX100 Copolyester
Eastman Tritan™ TX1000 Copolyester

PE8909 / 109251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.