MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Tritan™ GX100 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan copolyester GX100's strength, clarity and temperature resistance make it ideal for demanding applications. Extruded Sheet is manufactured with Eastman's Tritan copolyester GX100 resin in a thickness range from 0.080" to 0.250". It is readily available in clear with colors available upon request.

Application/Uses

  • Building and construction
  • Displays
  • Durables
  • Electronics
  • Signs
  • Transportation and outdoor vehicles

Key Attributes

  • Does not contain Bisphenol-A (BPA)
  • Does not contain plasticizers
  • Ease of fabrication
  • High impact
  • Temperature resistance
  • Thermoforming
  • Transparent

Information was provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Water Absorption 0.18 %
@Time 86400 sec
0.18 %
@Time 24.0 hour
Immersion; ASTM D570
Thickness 2970 microns117 milThickness of film tested; ASTM D374
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength at Break 46.0 MPa6670 psiASTM D638
Tensile Strength, Yield 45.0 MPa6530 psiASTM D638
Elongation at Break 133 %133 %ASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.483 GPa215.1 ksiASTM D790
Izod Impact, Notched  1.33 J/cm
@Temperature -30.0 °C
2.49 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 10.06 J/cm
@Temperature 0.000 °C
18.85 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 10.11 J/cm
@Temperature 23.0 °C
18.94 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  12.14 J/cm
@Temperature -30.0 °C
22.74 ft-lb/in
@Temperature -22.0 °F
ASTM D4812
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 99.2 °C211 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.9 °C196 °FASTM D648
Vicat Softening Point 110 °C230 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ FX100 Copolyester
Eastman Tritan™ MP100 Copolyester
Eastman Tritan™ EX401 Copolyester
Eastman Tritan™ FX200 Copolyester
Eastman Tritan™ TX1000 Copolyester

PE8910 / 109252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.