MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Claytone® 40 Rheological Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Claytone 40 is a modified montmorillonite designed to be used in aliphatic and aliphatic/aromatic systems that exhibit low to medium polarity. Claytone 40 functions as a thixotropic rheology modifier generating properties such as flow control and anti-setting. Claytone 40 provides reliable and reproducible rheological properties in solvent based paints, stains, enamels, primers, and inks as well as other applications. Claytone 40 requires the use of a polar activator to achieve full efficiency.

Applications:

  • Oil based paints and stains
  • Lubricating greases
  • Adhesives
  • Caulks and sealants
  • Cosmetics and personal care
  • Inks

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.545 - 0.641 g/cc0.0197 - 0.0231 lb/in³
Density 1.70 g/cc0.0614 lb/in³
Particle Mesh Size 200 Mesh200 Mesh70%
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 3.0 %3.0 %
Loss on Ignition(%) 36.5 - 40.5 %
@Temperature 1000 °C
36.5 - 40.5 %
@Temperature 1830 °F
 
Descriptive Properties
Color/FormVery light cream; Free flowing, finely divided powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Bentolite® L3 Magnesium aluminum Silicate Additive
BYK Claytone® EM Gellant for Oil Mud Systems
BYK Claytone® APA Rheological Additive
BYK Claytone® AF Rheological Additive
BYK Claytone® 409 Rheological Additive

PBYK021 / 185018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.