MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Bentolite® L3 Magnesium aluminum Silicate Additive
Categories: Ceramic; Clay

Material Notes: Bentolite L-3 is a specially processed magnesium aluminum silicate additive ideally suited for use as a binder and plasticizer for plastic refractory mixes. Its neutral pH and low impurity levels make it the best choice for mixes requiring long shelf life without loss of plasticity. In comparison with mixes containing conventional sodium bentonites. Bentlite L-3 plastic mixes maintain their tackiness, plasticity and shelf life for an extended period. Addition levels of 3-5% of Bentolite L-3 provide optimal binding and high green strength in high alumina phos-bonded mixes without harming the integrity of refractory properties.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.657 g/cc0.0237 lb/in³loose
 0.833 g/cc0.0301 lb/in³packed
Particle Mesh Size 200 Mesh200 Mesh80%
pH 7.57.52% slurry
 
Component Elements PropertiesMetricEnglishComments
Al2O3 14 %14 %
CaO 2.0 %2.0 %
Fe2O3 1.0 %1.0 %
H2O, Water 10 %10 %
Iron, Fe <= 1.0 %<= 1.0 %Soluble
K2O <= 0.50 %<= 0.50 %
Loss on Ignition(%) 6.0 %6.0 %
MgO 3.0 %3.0 %
Na2O <= 0.50 %<= 0.50 %
SiO2 74 %74 %
TiO2 <= 0.50 %<= 0.50 %
 
Descriptive Properties
Cation Exchange Capacity100 meq/100g
Color/FormOff white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Bentolite® L Bentonite
BYK Bentolite® L10 Bentonite
BYK Claytone® 3 Organophilic Bentonite
BYK Bentolite® L-400 Bentonite
BYK Claytone® 40 Rheological Additive

PBYK012 / 185009

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.