MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Claytone® 3 Organophilic Bentonite
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Claytone 3, an organoclay, is recommended as a rheological additive in oil based fluids and drilling muds. Claytone 3 is a high quality thixotrope suitable for use in low aromatic oils and synthetic solvents. In addition to imparting excellent rheological properties, Claytone 3 increases the carrying capacity and hole cleaning capabilities of the mud. Additionally, temperature and emulsion stability will be increased and fluid loss decreased.

Uses & Advantages:

  • Use in low aromatic or synthetic oil based drilling muds requiring rheological modification.
  • Directed at fluids that utilize synthetic or low aromatic oils.
  • Use in oil muds that are to be used as packer fluids or for stabilizer of stored muds.
  • Available in either 50 lb. or 25 Kg bags.
  • Economical, convenient, and safe to handle, mix, and store.
  • Easily dispersed and free flowing.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.417 g/cc0.0150 lb/in³loose
Particle Mesh Size 200 Mesh200 Mesh85%
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 37 %
@Temperature 1000 °C
37 %
@Temperature 1830 °F
 
Descriptive Properties
Color/FormOff-White, Free Flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Bentolite® L Bentonite
BYK Bentolite® L3 Magnesium aluminum Silicate Additive
BYK Bentolite® L-400 Bentonite
BYK Bentolite® L10 Bentonite
BYK Claytone® 409 Rheological Additive

PBYK019 / 185016

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.