MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® S 1568 Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® S 1568 is a food grade, gel-type, strongly acidic cation exchange resin based on a styrene-divinylbenzene copolymer. The favorable kinetics allow a distinctly higher operating capacity as this applies to comparable ion exchange resins with a heterodisperse bead size distribution. A much better total capacity enables long cycle times with a low leakage and economic quantities of regenerants. Lewatit S 1568 is very suitable for:
  • the softening of aqueous solutions, specially of juices occurring in the production of sugar and pectin
  • the decationization of solutions of organic products, e.g. beets, sugar cane, starch sugar, glycerol, gelatin, food grade acids etc.
  • the production of amino acids e.g. lysine
Lewatit S 1568 provides the resin filling with the following features:
  • a high exchange capacities in the regeneration and loading processes
  • a very good utilization of the total capacity
  • a low demand for wash water
  • a continuous flow of regeneration agents, water and solutions, equally shaped working zone
  • an almost linear pressure loss gradient along the whole bed depth, therefore and operation at higher bed depths is possible
  • an outstanding separation of components in the mixed bed filter.
If using Lewatit S 1568 for treating potable water and the a.m. aqueous solutions, you have to follow our recommendations for the start-up which are available on request.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.830 g/cc0.0300 lb/in³
Density 1.28 g/cc0.0462 lb/in³
Bead Size 0.550 - 0.650 mm0.0217 - 0.0256 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceDark brown
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Glycerin (HOCH2(CHOH)CH2O2CCH3; Glycerol)
Lanxess LEWATIT® S 1668 Cation Exchange Resin
LyondellBasell Adstif HA 1152 Polypropylene
Lanxess LEWATIT® S 6368 A OH Anion Exchange Resin
Lanxess LEWATIT® S 2528 Cation Exchange Resin

PLANY8820 / 209212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.