MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® S 2528 Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® S 2528 is a food grade, macroporous, strongly acidic cation exchange resin based on a styrene-divinylbenzene copolymer. It is bead-shaped and has a special bead size distribution for a use in the following processes:
  • Lewatit WS system (fluidized bed)
  • Lewatit VWS system (compound fluidized bed)
  • Standard co current regenerated system
Lewatit S 2528 is suitable for:
  • the decationization of solutions of organic products, e.g. sugar beet, sugar cane, starch sugar, and of the solutions of organic products, e.g. glycerin, gelatin, whey etc..
  • the softening of thin juice, e.g. Gryllus process in the sodium form
  • the removal of alkali ions for B-green e.g. Quentin process.
The macroporous structure of Lewatit S 2528 facilitates the adsorption of hydrophilic high molecular cationic organic substances. The organic substances, e.g. colorants, can easily be desorbed by regeneration with caustic soda solutions. If using Lewatit S 2528 to treat potable water and aqueous solutions listed above, special care should be given to the initial cycles of the new resin.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.760 g/cc0.0275 lb/in³
Density 1.27 g/cc0.0459 lb/in³
Bead Size 0.500 - 0.600 mm0.0197 - 0.0236 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceBeige-grey, opaque
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unipetrol Hydrogenated Refined Fermentative Ethanol Specially Denatured
Raschig Group MELOPLAS® 181 MF
Lanxess LEWATIT® S 1568 Cation Exchange Resin
Glycerin (HOCH2(CHOH)CH2O2CCH3; Glycerol)
Collagen

PLANY8823 / 209215

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.