MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Glycerin (HOCH2(CHOH)CH2O2CCH3; Glycerol)
Categories: Fluid; Solvent

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.2613 g/cc
@Temperature 20.0 °C
0.045567 lb/in³
@Temperature 68.0 °F
Viscosity  934 cP
@Temperature 25.0 °C
934 cP
@Temperature 77.0 °F
 1459 cP
@Temperature 20.0 °C
1459 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 92.11 g/mol92.11 g/mol
Surface Tension 63.4 dynes/cm
@Temperature 20.0 °C
63.4 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 66.9 bar50200 torr
Critical Temperature 453 °C847 °F
Critical Density 0.361 g/cc0.0130 lb/in³
Critical Molar Volume 255 cm³/mol15.6 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 42.542.5
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 198.7 J/g85.47 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 662.3 J/g284.9 BTU/lbEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 1.251 J/g-°C
@Temperature 25.0 °C
0.2990 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.292 W/m-K
@Temperature 25.0 °C
2.03 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Melting Point 18.1 °C64.6 °FAt atmospheric pressure (760 torr)
Boiling Point 290 °C
@Pressure 0.101 MPa
554 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4746
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.4746
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter17.2392
Antoine's Vapor Pressure B Parameter4487.04
Antoine's Vapor Pressure C Parameter-140.2
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)56-81-5
Chemical FormulaC3H8O3
Critical Compressibility (Zc)0.28
Dipole moment (p/C.m)1.001E-27
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A3337.1
Dynamic Viscosity Parameter B406
Molar Heat Capacity (298K)115.196 J/mol-K
Molar Heat Capacity of Vapor a Parameter8.4182
Molar Heat Capacity of Vapor b Parameter0.4439
Molar Heat Capacity of Vapor c Parameter-0.0003157
Molar Heat Capacity of Vapor d Parameter9.372E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UV cut-off (nm)207

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexane (C6H14)
Lanxess LEWATIT® S 1568 Cation Exchange Resin
Borosilicate Glass
LyondellBasell Adstif HA 1152 Polypropylene
Benzene (C6H6)

VORG024 / 74535

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.