MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlthane® 11T75D is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, with extremely high hardness. It is especially recommended for use in producing technical parts by injection molding.

Applications: Pearlthane 11T75D can be used for injection molding of a variety of technical parts. It can also be applied as base resin for extremely tough (glass reinforced) engineering compounds.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccISO 1183
Water Absorption 0.21 %ASTM D 570
Linear Mold Shrinkage 0.0020 cm/cmASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ISO 868
 80ISO 868
Tensile Strength at Break 50.0 MPaISO 527-2/1A/5
Tensile Strength, Yield 60.0 MPaISO 527-2/1A/5
Elongation at Break 230 %ISO 527-2/1A/5
Elongation at Yield 6.0 %ISO 527-2/1A/5
Modulus of Elasticity 2.17 GPaISO 527-2/1A/5
Flexural Strength 81.0 MPaISO 178
Flexural Modulus 2.27 GPaISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1 A
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1 A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 49.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °CISO 75
Vicat Softening Point 59.0 °CISO 360
Glass Transition Temp, Tg 39.0 °C
 
Processing PropertiesOriginal ValueComments
Zone 1 215 °C
Zone 2 220 °C
Zone 3 225 °C
Zone 4 225 °C
Adapter Temperature 225 °C
Die Temperature 225 °C
 225 °C
Drying Temperature 100 °C
@Time 10800 - 14400 sec
Dew Point -40.0 °C
 
Descriptive Properties
Compression Zone Temperature428°F
Metering Zone Temperature437°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU) (Extended Aging Data)
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer

PMEQU975 / 109212

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.