MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This grade has been specially designed for mechanically demanding applications where excellent mechanical properties are required, such as timing belts.

Information provided by Merquinsa.

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
10 g/10 min
@Load 47.6 lb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Tensile Strength, Yield 39.57 MPa5739 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
100% Modulus 8.012 MPa
@Strain 100 %
1162 psi
@Strain 100 %
ASTM D412
300% Modulus 16.63 MPa
@Strain 300 %
2412 psi
@Strain 300 %
ASTM D412
Tear Strength 112 kN/m639 pliASTM D624 DIE C
Abrasion 3030[mm^3]; DIN 53.516
 
Thermal PropertiesMetricEnglishComments
Melting Point 183 - 193 °C361 - 379 °FMQSA 114
Glass Transition Temp, Tg -40.0 °C-40.0 °FDSC, 50°F/min; DIN 51.007
 
Processing PropertiesMetricEnglishComments
Feed Temperature 196 °C385 °F
Nozzle Temperature 210 °C410 °F
Zone 1 191 - 199 °C375 - 390 °F
Zone 2 196 - 210 °C385 - 410 °F
Zone 3 199 - 216 °C390 - 420 °F
Zone 4 199 - 221 °C390 - 430 °F
Die Temperature 191 - 210 °C375 - 410 °F
Mold Temperature 35.0 °C95.0 °F
Moisture Content <= 0.10 %<= 0.10 %MQSA 44

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer

PMES80 / 101412

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.