MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M 941 Adhesive Transfer Tapes with Adhesive 100
Categories: Polymer; Adhesive

Material Notes: These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear values even at elevated temperatures. They also offer low “outgassing” properties, which is an important consideration for the aerospace, automotive and electronic industries

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.30 mil
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.50 pliHigh Surface Energy Plastic (ABS), Ultimate bond, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
 2.75 pliHigh Surface Energy Plastic (ABS), 20 min dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
 3.3125 plito Stainless Steel, 20 min dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
 3.375 pliHigh Surface Energy Plastic (ABS), 72 hr. dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
 4.875 plito Stainless Steel, 72 hr. dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
 9.0625 plito Stainless Steel, Ultimate bond, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
Insulation Resistance >= 9.40e+10 ohmCycle #410, test voltage = 100 VDC, MIL-I-46058C
 >= 1.50e+11 ohmCycle #4, test voltage = 100 VDC, MIL-I-46058C
 >= 9.70e+12 ohm24 hr after moisture resistance
 >= 1.00e+15 ohmBefore moisture resistance, test voltage = 100 VDC, MIL-I-46058C
Dielectric Constant 2.92
@Frequency 1000 Hz
ASTM D-150-92
Dielectric Strength 1100 kV/in500 vac, rms. [60 Hz]/sec; ASTM D149-92
Dissipation Factor 0.0025
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.9 µm/m-°C
@Temperature 125 - 175 °C
First heat; ASTM-D696
 58.4 µm/m-°C
@Temperature 25.0 - 175 °C
Second heat; ASTM-D696
Thermal Conductivity 0.178 W/m-K
@Temperature 51.0 °C
ASTM C518
 0.183 W/m-K
@Temperature 71.0 °C
ASTM C518
 0.187 W/m-K
@Temperature 101 °C
ASTM C518
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Liner58# Polycoated Kraft - 4.0 mils thick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9472 Adhesive Transfer Tapes with Adhesive 300
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471 Adhesive Transfer Tapes with Adhesive 300

PMM33203 / 167950

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.