MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9472 Adhesive Transfer Tapes with Adhesive 300
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive family is available in several thicknesses for a wide variety of surface bonding and provides a variety of liner configurations to help ensure excellent process flexibility.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 88.9 microns3.50 milLiner
 127 microns5.00 milAdhesive
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.60259 kN/m3.4375 pliPolypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
 0.66833 kN/m3.8125 pliPolypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
 0.8984 kN/m5.125 pliPolycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
 1.074 kN/m6.125 pliStainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
 1.249 kN/m7.125 pliStainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
 1.249 kN/m7.125 pliPolycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.21
@Frequency 1000 Hz
3.21
@Frequency 1000 Hz
0.040 thickness; ASTM D-150-92
Dielectric Strength 13.4 kV/mm
@Thickness 0.0508 mm
340 kV/in
@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
Dissipation Factor 0.040
@Thickness 0.0508 mm
0.040
@Thickness 0.00200 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 58.0 µm/m-°C32.2 µin/in-°FSecond heat; ASTM-D696
 20.0 µm/m-°C
@Thickness 0.0508 mm
11.1 µin/in-°F
@Thickness 0.00200 in
First heat; ASTM-D696
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Adhesive Type300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471 Adhesive Transfer Tapes with Adhesive 300
3M 9462P Adhesive Transfer Tapes with Adhesive 100

PMM33234 / 167981

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.