MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chosun Refractories CT-140S Fireclay Castables
Categories: Ceramic

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.002943 - 0.006867 GPa
@Temperature 1000 °C,
Time 10800 sec
 0.002943 - 0.007848 GPa
@Temperature 1350 °C,
Time 10800 sec
 0.003924 - 0.008829 GPa
@Temperature 110 °C,
Time 86400 sec
Compressive Strength 200 - 300 kg(f)/cm²
@Treatment Temp. 1000 °C,
Time 10800 sec
Cold Crushing Strength
 250 - 350 kg(f)/cm²
@Treatment Temp. 1350 °C,
Time 10800 sec
Cold Crushing Strength
 300 - 400 kg(f)/cm²
@Treatment Temp. 110 °C,
Time 86400 sec
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.001251 cal cm/sec-cm²-°C
@Temperature 260 °C
 0.0015568 cal cm/sec-cm²-°C
@Temperature 540 °C
 0.0018626 cal cm/sec-cm²-°C
@Temperature 800 °C
Maximum Service Temperature, Air 1400 °Climited
Shrinkage -1.20 %
@Temperature 1350 °C,
Time 10800 sec
 -0.0900 %
@Temperature 110 °C,
Time 86400 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 43 %
SiO2 44 %
 
Descriptive Properties
Installation MethodCasting, Troweling
Material Required for Estimating (kg/m3)2,000
Water Required for Casting(%)11.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chosun Refractories HACT-155 High Alumina Castables
Chosun Refractories HACT-180 High Alumina Castables
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens

CCHOS156 / 124100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.