MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.010791 GPa
@Temperature 110 °C,
Time 86400 sec
1.5651 ksi
@Temperature 230 °F,
Time 24.0 hour
 0.011772 GPa
@Temperature 1000 °C,
Time 10800 sec
1.7074 ksi
@Temperature 1830 °F,
Time 3.00 hour
 0.012753 GPa
@Temperature 1500 °C,
Time 10800 sec
1.8497 ksi
@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength  63.7 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
9250 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 66.7 MPa
@Treatment Temp. 1000 °C,
Time 10800 sec
9670 psi
@Treatment Temp. 1830 °F,
Time 3.00 hour
Cold Crushing Strength
 80.4 MPa
@Treatment Temp. 1500 °C,
Time 10800 sec
11700 psi
@Treatment Temp. 2730 °F,
Time 3.00 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1700 °C3090 °Flimited
Shrinkage  -0.400 %
@Temperature 1500 °C,
Time 10800 sec
-0.400 %
@Temperature 2730 °F,
Time 3.00 hour
 -0.0500 %
@Temperature 110 °C,
Time 86400 sec
-0.0500 %
@Temperature 230 °F,
Time 24.0 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 600 min2.00 - 10.0 hourSetting Time
 
Component Elements PropertiesMetricEnglishComments
Al2O3 75 %75 %
CaO 2.0 %2.0 %
SiO2 20 %20 %
 
Descriptive Properties
Installation MethodVibrating, Casting
Material Required for Estimating (kg/m3)2,750
Water Required for Casting(%)6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec RK 87 Alumina, 99.8%
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC)
Chosun Refractories HACT-155 High Alumina Castables
Chosun Refractories HACT-180 High Alumina Castables

CCHOS165 / 124109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.