MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chosun Refractories HACT-155 High Alumina Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.0024525 - 0.0063765 GPa
@Temperature 1000 °C,
Time 10800 sec
0.35571 - 0.92485 ksi
@Temperature 1830 °F,
Time 3.00 hour
 0.002943 - 0.006867 GPa
@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.9960 ksi
@Temperature 2460 °F,
Time 3.00 hour
 0.002943 - 0.006867 GPa
@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi
@Temperature 230 °F,
Time 24.0 hour
Compressive Strength  14.7 - 24.5 MPa
@Treatment Temp. 1000 °C,
Time 10800 sec
2130 - 3560 psi
@Treatment Temp. 1830 °F,
Time 3.00 hour
Cold Crushing Strength
 19.6 - 29.4 MPa
@Treatment Temp. 1350 °C,
Time 10800 sec
2840 - 4270 psi
@Treatment Temp. 2460 °F,
Time 3.00 hour
Cold Crushing Strength
 19.6 - 29.4 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
2840 - 4270 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.74442 W/m-K
@Temperature 260 °C
5.1579 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.84910 W/m-K
@Temperature 540 °C
5.8832 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.9305 W/m-K
@Temperature 800 °C
6.447 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Maximum Service Temperature, Air 1550 °C2820 °Flimited
Shrinkage  -0.0600 %
@Temperature 110 °C,
Time 86400 sec
-0.0600 %
@Temperature 230 °F,
Time 24.0 hour
 0.50 %
@Temperature 1350 °C,
Time 10800 sec
0.50 %
@Temperature 2460 °F,
Time 3.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 48 %48 %
SiO2 44 %44 %
 
Descriptive Properties
Installation MethodCasting, Troweling
Material Required for Estimating (kg/m3)2,150
Water Required for Casting(%)11.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories HACT-180 High Alumina Castables
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens
Chosun Refractories SAL90C Special High Alumina brick
Chosun Refractories CT-140S Fireclay Castables

CCHOS153 / 124097

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.