MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Teijin® Tetoron® SLA Polyester Film, 500 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Teijin® Tetoron® SLA is a super low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Teijin® Tetoron® SLA has achieved one of the lowest thermal shrinkage characteristics with superior flatness. Teijin® Tetoron® SLA has a lower shrinkage than Teijin® Tetoron® SL. It has a slightly hazy appearance.

Typical Applications: Teijin® Tetoron® SLA is suitable for use in many electrical applications where super low thermal shrinkage and superior flatness are very critical, but low haze is not required. Teijin® Tetoron® SLA is recommended for Flexible Printed Circuits (FPC) and Membrane Touch Switches (MTS).

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 5.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 190 %ASTM D882A
Film Elongation at Break, TD 130 %ASTM D882A
Film Tensile Strength at Break, MD 28000 psiASTM D882A
Film Tensile Strength at Break, TD 34000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD <= 0.10 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.00 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 150 Gauge
DuPont Teijin Films Mylar® LB Polyester Film, 48 Gauge (12 µm)
DuPont Teijin Films Mylar® 50 CL Polyester Film, Cap Liner and Ovenable Lidding, Heat Sealable, 50 Gauge
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 63 Gauge
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge

PDTZ9481 / 139798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.