MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 63 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.

This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This product is used for release films and is available in 500 gauge.

Typical Applications:

  • Tracing Film
  • Labels
  • Stamping
  • Imaging

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 16.0 microns0.630 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 90 %90 %ASTM D882A
Film Elongation at Break, TD 70 %70 %ASTM D882A
Coefficient of Friction, Dynamic 0.280.28ASTM D1894
Coefficient of Friction, Static 0.330.33ASTM D1894
Film Tensile Strength at Break, MD 186.0 MPa26970 psiASTM D882A
Film Tensile Strength at Break, TD 224.94 MPa32625 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 3.0 %
@Temperature 100 °C,
Time 1800 sec
3.0 %
@Temperature 212 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD -0.400 %
@Temperature 100 °C,
Time 1800 sec
-0.400 %
@Temperature 212 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 63 %63 %ASTM D1003
Transmission, Visible 78 %78 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® M34 Polyester Film, 50 Gauge (13 µm), PVDC Coated
DuPont Teijin Films Mylar® LB Polyester Film, 48 Gauge (12 µm)
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 150 Gauge
DuPont Teijin Films Teijin® Tetoron® SLA Polyester Film, 500 Gauge
DuPont Teijin Films Mylar® 50 CL Polyester Film, Cap Liner and Ovenable Lidding, Heat Sealable, 50 Gauge

PDTZ9489 / 139806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.