MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 gauge.

Approvals: UL 94 VTM-2 - 100 - 1000 gauge (0.025 - 0.25 mm) and UL Component Registration (RTI = 180/160°C) - Relative Thermal Index (RTI) = 180°C (Elect), 160°C (Mech)

Also available in 1000 Gauge

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³JIS C-2151
Moisture Absorption at Equilibrium 0.30 %0.30 %TDF Method
Water Vapor Transmission 104 g/m²/day6.70 g/100 in²/dayJIS Z0208
Thickness 12.2 microns0.480 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 90 %90 %JIS C-2318 (Modified to TDF)
Film Elongation at Break, TD 85 %85 %JIS C-2318 (Modified to TDF)
Coefficient of Friction, Dynamic 0.300.30JIS C2151
Coefficient of Friction, Static 0.300.30JIS C2151
Film Tensile Strength at Break, MD 276 MPa40000 psiJIS C-2318 (Modified to TDF)
Film Tensile Strength at Break, TD 262 MPa38000 psiJIS C-2318 (Modified to TDF)
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmJIS C-2318
Surface Resistivity per Square 2.00e+17 ohm2.00e+17 ohmJIS C-2151
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
JIS C-2318
 2.9
@Frequency 1e+9 Hz
2.9
@Frequency 1e+9 Hz
JIS C-2318
 3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
JIS C-2318
Dielectric Strength 300 kV/mm7620 kV/inJIS C-2318
Dissipation Factor  0.0030
@Frequency 60 Hz,
Temperature 25.0 °C
0.0030
@Frequency 60 Hz,
Temperature 77.0 °F
JIS C-2318
 0.0050
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.0050
@Frequency 1e+6 Hz,
Temperature 77.0 °F
JIS C-2318
 0.0050
@Frequency 1e+9 Hz,
Temperature 25.0 °C
0.0050
@Frequency 1e+9 Hz,
Temperature 77.0 °F
JIS C-2318
 
Thermal PropertiesMetricEnglishComments
Melting Point 269 °C516 °FDSC
Glass Transition Temp, Tg 121 °C250 °FDSC
UL RTI, Electrical 160 °C320 °F
UL RTI, Mechanical without Impact 180 °C356 °F
Shrinkage, MD 0.40 %
@Temperature 150 °C
0.40 %
@Temperature 302 °F
JIS C-2318 (Modified to TDF)
 2.0 %
@Temperature 200 °C,
Time 600 sec
2.0 %
@Temperature 392 °F,
Time 0.167 hour
Unrestrained
Shrinkage, TD 0.00 %
@Temperature 150 °C
0.00 %
@Temperature 302 °F
JIS C-2318 (Modified to TDF)
 1.0 %
@Temperature 200 °C,
Time 600 sec
1.0 %
@Temperature 392 °F,
Time 0.167 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %JIS K6714
Transmission, Visible 82 %82 %JIS K6714
UV Transmittance 8.0 %
@Wavelength 360 nm
8.0 %
@Wavelength 360 nm
TDF Method
 
Descriptive Properties
Coefficient of Hygroscopic Expansion0.000011/%RHTDF Method
F519 kpsiTD, TDF Method
 19 kpsiMD, TDF Method
Surface Roughness13/11 nmTDF Method (Inside/Outside)
Tear Propagation1.3 lbMD, TDF Method
 1.3 lbTD, TDF Method
Wettability (water angle)70°TDF Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Teonex® Q83 Polyester Film, 200 Gauge
DuPont Teijin Films Teonex® Q72 Polyester Film, 14 Gauge
DuPont Teijin Films Teonex® Q65FA
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness

PDTZ9497 / 139814

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.