MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis LE6025 Polyethylene Modified Jacketing Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: LE6025 is a black low density copolymer modified polyethylene compound. It is characterized by excellent stress crack resistance and mechanical properties and low temperature performance in combination with good extrudability. LE6025 contains 2,5% well dispersed furnace black of nominal particle size less than 25 nanometers in order to ensure excellent weathering resistance. Applications: Jacket for energy and communication cables. Specifications: ASTM D1248 Type I, Class C, Category 5, Grade E5, J3, W2-4; EN 50290-2-24; HD 620 S1, DMP 10, 12, 14, 17; HD 603 S1, DMP 7, 8; ISO 1872-PE, KCHL, 18-D003; and IEC 60502, Part 2, Type ST3.

Information provided by Borealis AG

Key Words: LDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccbase resin; ISO 1183
 0.933 g/cccompound; ISO 1183
ESCR 100% Igepal® >= 2500 hour
@Temperature 50.0 °C
F20; IEC 60811-4-1/B
Melt Flow 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 501s; ISO 868
Tensile Strength at Break >= 25.0 MPa50mm/min; ISO 527
Elongation at Break >= 900 %50m/min; ISO 527
Flexural Modulus 300 MPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmDC; IEC 60093
Dielectric Strength 20.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis LE6023 Polyethylene Modified Jacketing Compound
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive
Borealis LR4201R Polyethylene Insulation Compound, Crosslinkable
Borealis LE6022 Polyethylene Modified Jacketing Compound
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable

PBOREA522 / 108781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.