MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Desmopan® 460 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: injection molding grade; grease and oil-resistant; low compression set; good heat resistance; high elasticity; short cycle times; Application; Automotive engineering; Technical parts; Bearing bushes

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9797ISO 868
Hardness, Shore D 5959ISO 868
Tensile Strength, Ultimate 42.5 MPa6160 psi200 mm/min; DIN 53504
Tensile Stress at Strain  15.1 MPa
@Strain 10 %
2190 psi
@Strain 10 %
200 mm/min; DIN 53504
 22.5 MPa
@Strain 50 %
3260 psi
@Strain 50 %
200 mm/min; DIN 53504
 35.1 MPa
@Strain 100 %
5090 psi
@Strain 100 %
200 mm/min; DIN 53504
Elongation at Break 390 %390 %200 mm/min; DIN 53504
Tensile Modulus  0.130 GPa
@Temperature 60.0 °C
18.9 ksi
@Temperature 140 °F
ISO 6721-1,-4
 0.446 GPa
@Temperature 20.0 °C
64.7 ksi
@Temperature 68.0 °F
ISO 6721-1,-4
 1.75 GPa
@Temperature -20.0 °C
254 ksi
@Temperature -4.00 °F
ISO 6721-1,-4
Flexural Modulus 0.170 GPa24.7 ksi2 mm/min; ISO 178
Rebound 35 %35 %Resilience; ISO 4662
Tear Strength 150 kN/m856 pli500 mm/min; ISO 34-1
Abrasion 4040Method A; ISO 4649
Compression Set  21 %
@Temperature 70.0 °C,
Time 86400 sec
21 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 25 %
@Temperature 23.0 °C,
Time 259000 sec
25 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 32 %
@Temperature 70.0 °C,
Time 86400 sec
32 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 235 - 245 °C455 - 473 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 110 °C230 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 487 Thermoplastic Polyurethane
Covestro Desmopan® 392 Thermoplastic Polyurethane
Covestro Desmopan® 150 Thermoplastic Polyurethane
Covestro Desmopan® 385 Thermoplastic Polyurethane
Kolon KOPEL® KP3372 General Purpose TPE Resin

PBA107 / 26701

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.