MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Desmopan® 487 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Injection molding grade; grease and oil-resistant; low compression set; good heat resistance; short cycle times; Application; Automotive engineering; roller coating; Seals, membranes; Damping elements

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0432 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ISO 868
Hardness, Shore D 3333ISO 868
Tensile Strength, Ultimate 41.8 MPa6060 psiDIN 53504; DIN 53504
Tensile Stress at Strain  1.60 MPa
@Strain 10 %
232 psi
@Strain 10 %
DIN 53504; DIN 53504
 4.50 MPa
@Strain 50 %
653 psi
@Strain 50 %
DIN 53504; DIN 53504
 5.80 MPa
@Strain 100 %
841 psi
@Strain 100 %
DIN 53504; DIN 53504
 14.4 MPa
@Strain 300 %
2090 psi
@Strain 300 %
DIN 53504; DIN 53504
Elongation at Break 541 %541 %200 mm/min; DIN 53504
Tensile Modulus  0.0240 GPa
@Temperature 60.0 °C
3.48 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.0360 GPa
@Temperature 20.0 °C
5.22 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.183 GPa
@Temperature -20.0 °C
26.5 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Rebound 57 %57 %Resilience; ISO 4662
Tear Strength 84.0 kN/m479 pli500 mm/min; ISO 34-1
Abrasion 1212Method A; ISO 4649
Compression Set  13 %
@Temperature 23.0 °C,
Time 259000 sec
13 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 16 %
@Temperature 70.0 °C,
Time 86400 sec
16 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 23 %
@Temperature 70.0 °C,
Time 86400 sec
23 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 240 °C446 - 464 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® C 85 A HPM TPUR
Covestro Desmopan® 85786A Polyurethane
Covestro Desmopan® 385 Thermoplastic Polyurethane
Covestro Desmopan® 460 Thermoplastic Polyurethane
Covestro Desmopan® 392 Thermoplastic Polyurethane

PBA108 / 26702

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.